描述
METALLIZED POLYPROPYLENE

1206EFR-3-0.1-1-51 数据手册

 浏览型号1206EFR-3-0.1-1-51的Datasheet PDF文件第2页浏览型号1206EFR-3-0.1-1-51的Datasheet PDF文件第3页浏览型号1206EFR-3-0.1-1-51的Datasheet PDF文件第4页浏览型号1206EFR-3-0.1-1-51的Datasheet PDF文件第5页浏览型号1206EFR-3-0.1-1-51的Datasheet PDF文件第6页浏览型号1206EFR-3-0.1-1-51的Datasheet PDF文件第7页 
ELECTRONIC FILM CAPACITORS, INC.  
Reidville Industrial Park * 41 Interstate Lane  
WATERBURY, CONNECTICUT 06705  
PHONE (203) 755-5629  
FAX (203) 755-0659  
METALLIZED POLYPROPYLENE  
SERIES 1213  
EFC Series 1213 are metallized polypropylene capacitors. This series offers the advantage  
of superior stability, self healing, high insulation resistance, low dissipation factor and high  
frequency operation. Suggested applications include: timing circuits, switch mode power  
supplies (SMPS). Packaging options include: wrap and fill (TF, TC), radial lead box (EFR),  
axial lead (EC, EF). Application options include: switching power supply (SP).  
SPECIFICATIONS  
4. INSULATION RESISTANCE  
1. TEMPERATURE RANGE  
At 25 OC after 2 minutes charge time at rated voltage  
or 500 VDC, whichever is less, the minimum IR shall  
be 80,000 Megohm-Microfarads, but need not exceed  
120,000 Megohms.  
- 55 OC to + 85 OC at rated voltage.  
To 105 OC with 25% voltage derating.  
2. CAPACITANCE  
Capacitors < 1.0 MFD shall be measured  
_
at 1 KHz + 20 HZ. Capacitors >1.0 MFD  
5. HUMIDITY RESISTANCE  
Series 1213 shall meet the requirements  
of MIL-STD. 202C, Method 103B.  
shall be measured at 60 HZ. Measurements  
shall be taken at 25 OC.  
3. DIELECTRIC STRENGTH  
At 25 OC, 150% of rated voltage when applied  
terminal to terminal for one minute through a  
current limiting resistance.  
6. DISSIPATION FACTOR  
Shall be 0.1 % max. when measured as in Par. 2.  
7. LIFE TEST  
Will withstand the application of 150% rated voltage at +850C for 250 hours  
with not more than one failure in 12 permitted.  
TYPICAL TEMPERATURE CURVES  
METALLIZED POLYPROPYLENE  
CAPACITANCE CHANGE VS. TEMPERATURE  
DISSIPATION FACTOR VS. TEMPERATURE  
.15  
.10  
+2.0  
+1.0  
0
-1.0  
-2.0  
.05  
0
-3.0  
-4.0  
-55  
-25  
0
25  
50  
85  
105  
-55  
-25  
0
25  
50  
85  
105  
Temperature (OC)  
Temperature (OC)  
INSULATION RESISTANCE VS. TEMPERATURE  
7
10  
6
5
4
10  
10  
10  
3
10  
+25  
+50  
+85  
+105  
Temperature (OC)  

与1206EFR-3-0.1-1-51相关器件

型号 品牌 获取价格 描述 数据表
1206EFR-3-0.1-1-52 EFC

获取价格

METALLIZED POLYPROPYLENE
1206EFRA EFC

获取价格

Polypropylene and Foil Capacitors
1206EFRB EFC

获取价格

Polypropylene and Foil Capacitors
1206F102XXX ETC

获取价格

Multilayer Ceramic Chip Capacitors Products NPO, X7R, Y5V
1206F104XXX ETC

获取价格

Multilayer Ceramic Chip Capacitors Products NPO, X7R, Y5V
1206FA VMI

获取价格

200 V - 1,000 V Single Phase Bridge 3.0 A Forward Current 70 ns - 3000 ns Recovery Time
1206FB VMI

获取价格

200 V - 1,000 V Single Phase Bridge 3.0 A Forward Current 70 ns - 3000 ns Recovery Time
1206FC VMI

获取价格

200 V - 1,000 V Single Phase Bridge 3.0 A Forward Current 70 ns - 3000 ns Recovery Time
1206FD VMI

获取价格

200 V - 1,000 V Single Phase Bridge 3.0 A Forward Current 70 ns - 3000 ns Recovery Time
1206FE VMI

获取价格

200 V - 1,000 V Single Phase Bridge 3.0 A Forward Current 70 ns - 3000 ns Recovery Time