Multilayer Ceramic Capacitors
Approval Sheet
5. EXTERNAL DIMENSIONS & CONSTRUCTIONS
Size
Inch (mm)
L (mm)
W (mm)
T (mm)/Symbol
Remark
MB (mm)
L
0.25
+0.05/-0.10
0402 (1005)
E
S
#
1.00±0.20
0.50±0.20
0.50±0.20
0.80±0.07
T
1.60±0.20
1.60±0.30
0.80±0.10
0.80±0.30
0603 (1608)
0805 (2012)
0.40±0.15
0.50±0.20
0.80±0.30
0.60±0.10
0.80±0.10
1.25±0.10
1.25±0.30
0.80±0.10
X
A
B
D
I
W
MB
MB
2.00±0.20
2.00±0.30
1.25±0.10
1.25±0.30
#
#
Fig. 1 The outline of MLCC
B
0.95±0.10
1.15±0.15
1.25±0.10
1.60±0.20
1.60±0.50
0.95±0.10
C
J
#
#
#
#
#
#
3.20+0.4/-0.1
1.60±0.15
0.60±0.20
(0.50±0.25)*
1206 (3216)
1210 (3225)
D
G
P
C
3.20+0.4/-0.1
3.20±0.50
1.60±0.20
1.60±0.50
3.20±0.40
2.50±0.20
2.50±0.50
2.03±0.25
3.20±0.30
1.25±0.10
1.60±0.20
2.00±0.20
2.50±0.50
1.25±0.10
2.00±0.20
1.25±0.10
D
G
K
#
#
#
#
#
#
#
0.75±0.25
0.50±0.25
3.20±0.60
M
D
K
1808 (4520) 4.50+0.6/-0.4
D
1.60±0.20
2.00±0.20
2.50±0.50
G
K
#
#
#
#
#
0.75±0.25
(0.50±0.25)*
1812 (4532) 4.50+0.6/-0.4
1825 (4563) 4.50+0.6/-0.4
3.20±0.40
6.30±0.40
5.00±0.40
6.30±0.40
M
2.00±0.20 (K)
2.50±0.30 (M)
2.80±0.30 (U)
3.10±0.30 (R)
0.75±0.35
0.85±0.35
0.85±0.35
2220 (5750)
2225 (5763)
5.70±0.50
5.70±0.50
#
# Reflow soldering only is recommended.
* For 1206≧1000V, 1812_200V~4000V products.
6. GENERAL ELECTRICAL DATA
Dielectric
NP0
0402, 0603, 0805, 1206, 1210, 1808, 1812, 1825, 2220, 2225
0.1pF to 0.1μF 100pF to 47μF 0.033μF to 10μF
X7R
X5R
Size
Capacitance range*
Cap≤5pF:
B (±0.1pF), C (±0.25pF)
5pF<Cap<10pF:
C (±0.25pF), D (±0.5pF)
Cap≥10pF:
Capacitance tolerance**
K (±10%), M (±20%)
F (±1%), G (±2%),
J (±5%), K (±10%)
Rated voltage (WVDC)
Operating temperature
Capacitance characteristic
Termination
6.3V to 4000V
-55 to +125°C
-55 to +125°C
±30ppm
-55 to +85°C
±15%
±15%
Ni/Sn (lead-free termination)
* Measured at the condition of 30~70% related humidity.
NP0: Apply 1.0±0.2Vrms, 1.0MHz±10% for Cap≤1000pF and 1.0±0.2Vrms, 1.0kHz±10% for Cap>1000pF, 25°C at ambient temperature
X7R, X5R: Apply 1.0±0.2Vrms, 1.0kHz±10%, at 25°C am bient temperature.
** Preconditioning for Class II MLCC: Perform a heat treatment at 150±10°C for 1 hour, then leave in a mbient condition for 24±2 hours
before measurement.
Page 3 of 27
ASC_Soft termination_(SH)
Mar. 2024