MKT 370
DC Film Capacitors
MKT Radial Potted Type
Vishay BCcomponents
SUB-CLAUSE NUMBER AND TEST
CONDITIONS
PERFORMANCE REQUIREMENTS
4.9
Shock
Mounting:
See section “Mounting” of this specification
Pulse shape: Half sine
Acceleration: 490 m/s²
Duration of pulse: 11 ms
4.9.3
Final measurements
Visual examination
Capacitance
No visible damage
|ΔC/C| ≤ 3 % of the value measured in 4.6.1
Tangent of loss angle
Increase of tan δ
≤ 0.010 for:
C ≤ 220 nF or
≤ 0.015 for:
220 nF < C ≤ 470 nF and
≤ 0.003 for:
C > 470 nF
Compared to values measured in 4.6.1
Insulation resistance
As specified in section “Specific Reference
Data 370” of this specification
SUB-GROUP C1 COMBINED SAMPLE
OF SPECIMENS OF SUB-GROUPS
C1A AND C1B
4.10
Climatic sequence
4.10.2 Dry heat
Temperature:
+ 100 °C for rated voltage 63 V
+ 105 °C for rated voltage > 63 V
Duration: 16 h
4.10.3 Damp heat cyclic
Test Db, first cycle
4.10.4 Cold
Temperature: - 55 °C
Duration: 2 h
4.10.6 Damp heat cyclic
Voltage proof = URdc for 1 min within 15 min
after removal from testchamber
No breakdown of flash-over
Test Db, remaining cycles
4.10.6.2Final measurements
Visual examination
No visible damage
Legible marking
Capacitance
|ΔC/C| ≤ 5 % of the value measured in
4.4.2 or 4.9.3
Tangent of loss angle
Increase of tan δ
≤ 0.010 for:
C ≤ 220 nF or
≤ 0.015 for:
220 nF < C ≤ 470 nF and
≤ 0.005 for:
C > 470 nF
Compared to values measured in
4.3.1 or 4.6.1
Insulation resistance
≥ 50 % of values specified in section “Specific
Reference Data 370” of this specification
SUB-GROUP C2
4.11
Damp heat steady state
56 days, 40 °C, 90 % to 95 % RH
4.11.1 Initial measurements
Capacitance
Tangent of loss angle at 1 kHz
www.vishay.com
92
For technical questions, contact: dc-film@vishay.com
Document Number: 28108
Revision: 04-Aug-09